Colorful Paint Fake

2019-05-17

Phenomenon description

In the process of construction, the uneven distribution density of colored dots is inconsistent, and the effect of the sample is quite different。

Cause Analysis

1.Inconsistent brushing of the primer and leakage caused by partial anti-alkali;

2.The flatness of the substrate is poor;

3.Scaffolding construction produces more frame marks;

4 .did not follow the instructions for use, the product dilution ratio is too large;

5.One-time spraying too thick leads to product sag;

6.Use quality products with unqualified quality;

7.Different batches of products are used on the same wall;

8.Violent shaking, etc., so that the color point breaks and mixed colors。

Solution

1.Use a closed alkali-resistant primer with excellent performance and apply it as required;

2.The substrate should meet the requirements of intermediate plastering;

3.Try to use the hanging basket for construction;

4.In strict accordance with the use of products, it is strictly prohibited to add water to dilute;

5.The use of colorful paint should be used in multiple ways of spraying, the single-use construction consumption is recommended to be controlled below 0.4kg / m2;

6.Select products with qualified product quality for construction;

7.Different batches of products are strictly prohibited from being used on the same wall;

8.The colorful paint is strictly prohibited from being stirred vigorously before use. It can be mixed by using the method of pouring。

System products
Baojun colorful paint system



Home· BaoJun· Construction Coating· Industrial Coating· Solution· Project· Service· Intelligent Manufacturing

Address:No. 9 Chuangxin Avenue, Binhai Science and Technology Park, Binhai High-tech Zone, Tianjin,China Zip code:300457

National Hotline

400-022-5055

Copyright © 2019 BaoJunPaint.com All Rights Reserved. 版权所有 宝骏涂料 京ICP备12053088号-1